Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4827
Hi, We are observing solder joint discoloration ( yellow ... - Jan 04, 2019 by Ameen
Try to measure the profile again by datasheet..with the resu... - Jan 04, 2019 by Panaguru
Hi, Thanks for the valuable feedback. We are at lower ... - Jan 04, 2019 by Ameen
If I understood on that electronics, you have a bot and a to... - Jan 04, 2019 by Panaguru
Hi , thanks.. yes you are right.Its bot and top side. ... - Jan 04, 2019 by Ameen
we never used a paste of this type...not everything in the p... - Jan 04, 2019 by Panaguru
Hi, Here we take profile for every changeover. And we com... - Jan 04, 2019 by Ameen
Hi, I would like to try to help, but I think I need help ... - Jan 07, 2019 by Steve Thomas
Hi Steve, We did the below trials today. 1. Run the b... - Jan 08, 2019 by Ameen
Sounds like you're making progress! The one thing that y... - Jan 09, 2019 by Steve Thomas
Hi Steve, Thanks. This from the trusted supplier. ... - Jan 10, 2019 by Ameen
It's unlikely to be a reliability issue. It looks like tin ... - Jan 18, 2019 by SMTA-Timothy SMTA
Hi, Thanks for the valuable feedback. Thanks ALL. R... - Jan 18, 2019 by Ameen
cColor is NOT a measure of solder connection quality. It is ... - Jan 19, 2019 by davef
Thanks Dave, For the feedback. It was initially rejected ... - Jan 19, 2019 by Ameen
Have you tried to reduce the temperature for the second side... - Jan 19, 2019 by Panaguru
Hi, Thanks . It was ok with N2 environment. Reducin... - Jan 19, 2019 by Ameen
Lead free HASL coatings can be susceptible to yellowing duri... - Jan 21, 2019 by SMTA-Tony SMTA
Hi Tony, Thanks for the valuable feedback. We got to k... - Jan 21, 2019 by Ameen