Who's controlling the cooling rate when profiling? If so, w... - Jan 31, 2020 by dontfeedphils
We never really "controlled" it, per-se...more a f... - Feb 03, 2020 by robgd3
A few lifetimes ago I went to a seminar on reflow profiles. ... - Feb 03, 2020 by Stephen
Reason I ask is because I've never really paid much attentio... - Feb 03, 2020 by dontfeedphils
There are two areas that are important when discussing cooli... - Feb 04, 2020 by Fred Dimock
Hello Phil, As the other respondents have mentioned, the co... - Feb 10, 2020 by SMTA-Tony SMTA
on 10 zone ovens with 3 cooling zones, my negative slope is ... - Feb 10, 2020 by Evtimov
The ideal cooling zone curve should be a mirror image of the... - Apr 22, 2020 by SMTA-Samy SMTA