Hello all, I am randomly getting solder short due to voids ... - Jun 16, 2020 by Srini
Your statement is interesting, but not necessarily correct. ... - Jun 16, 2020 by Evtimov
Thanks for your response. Shorts are happening in differen... - Jun 16, 2020 by Srini
Voids form mainly two ways. 1. Contamination - due PCB pads... - Jun 16, 2020 by Evtimov
Point one -; I am also having this concern but based on the ... - Jun 16, 2020 by Srini
These are great pictures. I have never seen this kind of sol... - Jun 17, 2020 by Evtimov
Thank you for your valuable inputs. Current two SMT line is... - Jun 17, 2020 by Srini
I would say you check FAB drawing and see if there is any st... - Jun 18, 2020 by Evtimov
Usually board house should inform you of these. Here suppli... - Jun 18, 2020 by Srini
We also don't inspect any things in incoming PCBs. We have C... - Jun 19, 2020 by Srini
Hi SRINI, Are you able to show X-ray of these 2 locations fr... - Jun 30, 2020 by CPH
Hi CPH, Thanks for your response. Sure I will share. But g... - Jun 30, 2020 by Srini
Few more images attached. ... - Jul 07, 2020 by Srini
Interesting!. They don't look like voids as usual meanings. ... - Jul 08, 2020 by DucHoang
Hi DucHoang, Thanks for the response. I will share the im... - Jul 08, 2020 by Srini
OSP board finish is the issue. With OSP microBGA board, we n... - Jul 08, 2020 by DucHoang
Thanks for your input. I do understand from this thread tha... - Jul 08, 2020 by Srini
Hi, Image 1 - Solder short image Image 2 Same component X r... - Jul 10, 2020 by Srini
The bubble inside BGA ball locate at via in pad and apply th... - Jul 11, 2020 by researchmfg
Thanks for your valuable inputs. I will work to apply resin... - Jul 11, 2020 by Srini
We are currently running different make PCB and no such kind... - Jul 31, 2020 by Srini
That was the most logical. I am glad you solved it. ... - Jul 31, 2020 by Evtimov
Good to hear problem has gone. ... - Aug 02, 2020 by researchmfg
Could you please enlight me on how to prove the issues by us... - Aug 04, 2020 by Srini