Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Just wondering what everyone's ideas are on the best cleanin... - Mar 22, 2004 by jdumont
Residues from what type of flux are you cleaning? ... - Mar 25, 2004 by davef
No clean and RMA, both R0L0. Is it true that RMA type pastes... - Mar 26, 2004 by jdumont
Dear Sir, If you are looking for the best bang for the bu... - Mar 26, 2004 by Patrick Bruneel
Patrick, When you say "no-residue" what exactly do you me... - Mar 26, 2004 by
Id also like to know how this is possible. I am skeptical an... - Mar 26, 2004 by jdumont
jdomont, No-cleans are more difficult to clean than RMA�s... - Mar 26, 2004 by
Hi Patrick, With all due respect, it is easy to quantify ... - Mar 26, 2004 by
Mr. Dumont I want to be very clear on a couple of points.... - Mar 26, 2004 by Patrick Bruneel
Big Claims� No Data� Ummm� ... - Mar 26, 2004 by Michael
Patrick, can't you just post the data? I noticed it wasn't ... - Mar 26, 2004 by RDR
Hi, I would also be interested in this thread, but our pr... - Mar 28, 2004 by
We are also having the same problem here. I was told earlier... - Mar 29, 2004 by jdumont
Patrick, I would like to try a sample of your product. Pleas... - Mar 29, 2004 by jdumont
Thanks Josh, email your company name, address and phone N... - Mar 29, 2004 by Patrick Bruneel
Grant & JDumont: You should not have this white residue o... - Mar 29, 2004 by davef
Hi Dave, its not the connections that have the white residue... - Mar 29, 2004 by jdumont
The only time I have ever had this happen was with un/not fu... - Mar 29, 2004 by RDR
Russ is correct. ... - Mar 29, 2004 by davef
Well how can I correct this? Would baking the board prior to... - Mar 29, 2004 by jdumont
Josh: Final cure of the LPI solder mask: 310*F for 45 minute... - Mar 29, 2004 by davef
Hi, Thanks for the ideas. With the solder mask curing pro... - Mar 30, 2004 by
If you can rub it off, it's unlikely to be a solder mask pro... - Mar 30, 2004 by davef
Hey guys. I've been manually dunking circuit boards for 8 y... - Mar 31, 2004 by
Deltawave flux pump continously runs while in run mode. Afte... - Apr 01, 2004 by
Hi, Thanks for the info. How clean can wave soldering get... - Apr 02, 2004 by
Hi, We tried that, as the Soltec has a spray fluxer that ... - Apr 02, 2004 by
Hi, We have the spray fluxer, and I will have a look for ... - Apr 02, 2004 by
Take a look at the downloadable paper on the subject of "Whi... - Apr 02, 2004 by
White residue can often be caused by overheating the flux. W... - Apr 02, 2004 by
Hi, Thanks for the tip, and I will check that out! We hav... - Apr 05, 2004 by