NexLev Open Solder and Hyper BGA

Andrew

#29783

NexLev Open Solder and Hyper BGA | 1 August, 2004

I am seeing high rate of open joint at NexLev connector and also BGA warpage issue with 52 mm Hyper BGA.anyone has the same experience?

reply »

#29828

NexLev Open Solder and Hyper BGA | 4 August, 2004

We assume your opens are on the corners. If so, you are screwed.

Look here: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=28669

reply »