Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Lead Free Ball Grid Array packages are expected to be increa... - Feb 18, 2005 by ABHI
Hi, The normal electronic components you purchase should ... - Feb 18, 2005 by
Currently, we see lead-free solderballs on BGA. The issue f... - Feb 19, 2005 by davef
Thanks Grant and Dave. I have done extensive work on this... - Feb 21, 2005 by ABHI
We're try to stay away from using electroless nickel. Pleas... - Feb 21, 2005 by davef
Davef, We see increased IMC thickness for electroless Ni and... - Feb 21, 2005 by ABHI
It could be that you're starting with hyper corroded nickel,... - Feb 22, 2005 by davef