Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi, We are trying to break a component ( SMT component ) ... - Mar 22, 2005 by
There is no standard. This is a relative test. If you wish ... - Mar 22, 2005 by davef
Sounds like EA has way too much free time on his hands. How ... - Mar 23, 2005 by
Hi, We are running the automotive product and question wa... - Mar 24, 2005 by
Hi davef, Appreciate your advise...... ... - Mar 24, 2005 by
So far I've been working with a xtal. I've been placing this... - Mar 28, 2005 by
chon, we do a similar kind of perpendicular test, but have... - Mar 29, 2005 by
Indy, Please refer to IPC-TM-650 TEST METHOD MANUAL Number ... - Mar 29, 2005 by
IPC-TM-650 TEST METHODS MANUAL Number 2.4.21.1 Subject: Bon... - Mar 29, 2005 by davef
Davef That's why I mentioned that this was the "Closest" w... - Mar 30, 2005 by
If there's no shear strength standard for solder joint, how ... - Mar 30, 2005 by
There is no spec because solder is designed to provide an el... - Mar 30, 2005 by URL
we also have a need to measure the solder bond strength of o... - Apr 04, 2005 by
EA