Dear all, We observed visible micro crack at top side of ... - Aug 01, 2005 by
Joseph, What is the topside temp reading of your board befor... - Aug 01, 2005 by kamran
Based on your description, it sounds like the solder connect... - Aug 01, 2005 by davef
We use SAC305 and top side particular joint temp. is 110 deg... - Aug 01, 2005 by
IPC-A-610D Section 5, shows a variety of photographs of: * ... - Aug 02, 2005 by davef
Yes, lead can promote fillet lift. In order to understand t... - Aug 03, 2005 by
Hello Joseph, Sorry for the bad news but microcracking is a... - Aug 10, 2005 by Robert Dervaes
Bob, Great theory if you're selling SN100C, but I have to... - Aug 10, 2005 by Patrick Bruneel
Joseph, In addition to my previous post The reason why t... - Aug 10, 2005 by Patrick Bruneel