Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 8576
Does anyone one have any suggestions on what containers to u... - Sep 27, 2005 by Steve Combs
Hi Steve, When I drain our wave solder pot in preparation fo... - Sep 27, 2005 by
Hi Jay, Have you used those methods before? The muffin tin ... - Sep 27, 2005 by Steve Combs
Contact your solder supplier and ask if you can borrow the m... - Sep 27, 2005 by
Use "Bakers Secret" Teflon coated loaf pans to make the nice... - Sep 27, 2005 by davef
your supplier should be able to provide you with all the nec... - Sep 28, 2005 by
Thanks to Stevezeva for hosting the pictures: Bakers Secr... - Sep 28, 2005 by
Yes, I've used the muffin tins. I drained a solder drag pot... - Sep 28, 2005 by
Thanks for everyones input. I'm sure others will find this ... - Sep 29, 2005 by Steve Combs
How do you drain out the solder at the bottom ? I thought mo... - Oct 04, 2005 by
Sure, using the drain for the last portion, that's difficult... - Oct 05, 2005 by davef
Just be prepared! Once you open the drain you may not be ... - Oct 05, 2005 by jdengler
Should be another thread but oh well, Marcus can you advise... - Oct 06, 2005 by RDR
With what did you compare the drossing against ? Sn/Pb or ... - Oct 06, 2005 by
Hi Marcus, how are you enjoing SN100 ? It seams the SN... - Feb 21, 2006 by