Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4145
Hello everybody, We are in the process of implementing NC... - Oct 01, 2005 by
Hiram
#36930
NC flux options | 1 October, 2005
Hello everybody,
We are in the process of implementing NC process on the wave solder. We have a Sonotek XL fluxing system. Any ideas out there?
Solder used: SN100C Flux options so far: 264-5 flux, 270WR VOC-free 9both from AIM solder)
The flux chosen must be also suitable for selective solder machine (solder bath)and lead-free compatible.
I appreciate you feedback as usual.