Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4840
Hi, We have a customer who give us a 20K board contract e... - Oct 13, 2005 by ING
Hi, What is the speed of the conveyir (contact time) and ... - Oct 14, 2005 by LUPO
For LUPO: speed: 4.5 inch alloy: 63Sn/37Pb Solder pot t... - Oct 14, 2005 by ING
According with temperature vs. wetting force diagram 245-2... - Oct 14, 2005 by LUPO
We have a simular problem with Ni/Au; especially whith pcb t... - Oct 14, 2005 by
Mika, 1.) Is there a maximum board thickness where it wou... - Oct 14, 2005 by Patrick Bruneel
Thanks Patrick, I our mixed standard HASL/RoHS production a... - Oct 14, 2005 by
Mika, If I understand you correctly you compare hole fill... - Oct 14, 2005 by Patrick Bruneel
Thanks Patrick for the replay, No, we do not mix the alloys... - Oct 14, 2005 by
I Am SORRY; I mean of corse ING. I must be tired, because I... - Oct 14, 2005 by
Thanks Patrick. I understand your points. It gives us go... - Oct 17, 2005 by ING
I suspect the problem is a surfactant issue in your flux. I ... - Oct 18, 2005 by