Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3473
Can anybody suggest that how we can chek quality for solderi... - Jan 07, 2006 by MSK
apply flux then dip the component into a solder pot. this wo... - Jan 09, 2006 by
You can find some good idea by reading IPC-J-STD-002B (or ... - Jan 09, 2006 by
Perhaps I read your question wrong, but I would be more incl... - Jan 09, 2006 by Steve Thomas
Thanks to all but my quistion is that with which instrument ... - Jan 11, 2006 by MSK
MSK As GS told you in an earlier posting, J-STD-002 and I... - Jan 11, 2006 by davef
We've got a Must II, and it works fine. The service in the U... - Jan 11, 2006 by Rob