Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5413
Hi All, I�ve been doing some research on the issue of run... - Jan 31, 2006 by carterhoward
how would you apply both pastes.? anyway, I have succesfu... - Jan 31, 2006 by aj
Today's regular Sn-Pb paste chemistries are designed to run ... - Jan 31, 2006 by
I guess my biggest concern would be what will happen to the ... - Jan 31, 2006 by carterhoward
We just did this and are awaiting the results. Solder balli... - Jan 31, 2006 by
Hi all, I'm working in Military Production and then, We hav... - Feb 01, 2006 by
Hi, SAC BGA's in a SnPb reflow process can be achieved by... - Feb 01, 2006 by Joe
Try an intermediate paste like Loctite/Henkle 218. It's des... - Feb 01, 2006 by
At my last employer, we ran a number of tests to make a "Hyb... - Feb 03, 2006 by
Mike did you have these SEM'd to be able to see the IMC's wi... - Feb 06, 2006 by
No we didnt. All our images where visual. ... - Feb 08, 2006 by