Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3861
Can someone point out what sort of defects at the joint I ca... - Feb 07, 2006 by
Hi, I would say the most worrying defect would be damaged... - Feb 07, 2006 by Grant
Hi, other effect could be the extra inter-metallic thickn... - Feb 07, 2006 by
'TAL' is a poor measure of solder connection heating. In a ... - Feb 08, 2006 by davef
DaveF is correct in saying that TAL is not the best metric t... - Feb 10, 2006 by
Wow, how people get off track. You'll probably see OK joint... - Feb 10, 2006 by
You will begin to de-wet at a high TAL and actually likely s... - Feb 13, 2006 by PeteC
Mike