Effects of Thermal Aging on Copper Dissolution For SAC 405 Alloy

Published:

July 8, 2010

Author:

Dr. Dana Medlin, Clay Voyles, Teneil Ryno, Casey Bergstrom, John Metzger, and Spencer Richards

Abstract:

Aging characteristics of new lead free solder alloys are in question by many experts because of higher amount of tin’s effect on the diffusion of other metals, primarily copper, to create undesirable boundary intermetallics over long periods of time and even moderately elevated temperatures. A primary layer of intermetallics, Cu6Sn5 forms as the liquid solder makes contact with the solid copper substrate. This reaction however ceases as the solder temperature falls below that of liquidus. A secondary intermetallic Cu3Sn1, an undesirable weak and brittle layer, is thought to form over time and may be accelerated by even mildly elevated temperatures in electronic modules such as laptops under power.

This project was designed to quantify the growth rate of Cu3Sn1 over an extended period of time in a thermal environment similar to a laptop in the power on mode....

  • Download Effects of Thermal Aging on Copper Dissolution For SAC 405 Alloy article
  • To read this article you need to have Adobe PDF installed

You must be a registered user to talk back to us.

 

Company Information:

Radiance Technologies, Inc. provides systems engineering and technology development services to the government. Its products

Huntsville, Alabama, USA

Other

  • Phone (256) 704-3400

See Company Website »

Company Postings:

(2) technical library articles

  • Apr 11, 2022 - iNEMI Webinar 07.07.2021 - PCB Cleaning | ZESTRON Americas
  • Jan 28, 2022 - Open Radio Unit White Box 5G | Whizz Systems
  • Nov 10, 2021 - Understanding the Cleaning Process for Automatic Stencil Printers | ITW EAE
  • Oct 20, 2021 - PCB Surface Finishes & The Cleaning Process - A Compatibility Study | ZESTRON Americas
  • Oct 06, 2021 - Cleaning Before Conformal Coating | ZESTRON Americas
  • Browse Technical Library »

Effects of Thermal Aging on Copper Dissolution For SAC 405 Alloy article has been viewed 461 times

Capillary Underfill process

Benchtop Fluid Dispenser