Intermetallic Growth in Tin-Rich Solders

Published:

June 13, 2017

Author:

Louis Zakraysek

Abstract:

For tin-rich solder alloys, 200 C (392 F) is an extreme temperature. Intermetallic growth in tin-copper systems is known to occur and is believed to bear a direct relationship to failure mechanisms. This study of morphological changes with time at elevated temperatures was made to determine growth rates of tin-copper intermetallics. Preferred growth directions, rates of thickening, and notable changes in morphology were observed.

Each of four tin-base alloys was flowed on copper and exposed to temperatures between 100 C and 200 C for time periods of up to 32 days. Metallographic sections were taken and the intermetallics were examined. Intermetallic layer thickening is characterized by several distinct stages. The initial growth of side plates is extremely rapid and exaggerated. This is followed by retrogression (spheroidization) of the elongated peaks and by general thick-...

  • Download Intermetallic Growth in Tin-Rich Solders article
  • To read this article you need to have Adobe PDF installed

You must be a registered user to talk back to us.

 

Company Information:

What makes GE great? According to a survey in FORTUNE magazine, GE is the most admired company in the world. We have great products and great processes, but most importantly, we have great people! To View Our Current Job Openings Please Visit Our Web

SCHENECTADY, New York, USA

Manufacturer, Other, Recruiter / Employment Company

  • Phone 518 385 4537
  • Fax 949-221-7931

See Company Website »

Company Postings:

(2) products in the catalog

(2) technical library articles

  • Apr 11, 2022 - iNEMI Webinar 07.07.2021 - PCB Cleaning | ZESTRON Americas
  • Jan 28, 2022 - Open Radio Unit White Box 5G | Whizz Systems
  • Nov 10, 2021 - Understanding the Cleaning Process for Automatic Stencil Printers | ITW EAE
  • Oct 20, 2021 - PCB Surface Finishes & The Cleaning Process - A Compatibility Study | ZESTRON Americas
  • Oct 06, 2021 - Cleaning Before Conformal Coating | ZESTRON Americas
  • Browse Technical Library »

Intermetallic Growth in Tin-Rich Solders article has been viewed 825 times

Jetting Pump for Integration

ICT Total SMT line Provider