ALD of Alumina Ceramic Films for Hermetic Protection
Published: |
August 5, 2020 |
Author: |
ACI Technologies, Inc. |
Abstract: |
A primary issue in electronics reliability for military applications is the ability to ensure long term operability in harsh, extreme environments. This requires more rigid standards, such as the MIL-STD-883 (Department of Defense Test Method Standard for Microcircuits), which commercial grade electronics typically do not satisfy. A solution commonly employed is to package the critical electronic components in hermetically sealed metal or ceramic enclosures which are costly and labor intensive. Not only are the components more expensive, but the assembly process is more difficult to automate, resulting in a substantial cost premium for military grade electronics.... |
You must be a registered user to talk back to us. |
Company Information:
More articles from ACI Technologies, Inc. »
- Dec 07, 2020 - A Non-destructive Approach to Identify Intermittent Failure Locations on Printed Circuit Cards (PCC) that have been Temperature Cycle Tested
- Nov 09, 2020 - Ball Grid Array (BGA) Voiding Affecting Functionality
- Sep 02, 2020 - Reworking ALD Coatings
- Jul 01, 2020 - Lead-Free Risk Mitigation -- A Case Study
- Jun 02, 2020 - Lead-Free Control Plan
- See all SMT / PCB technical articles from ACI Technologies, Inc. »
More SMT / PCB assembly technical articles »
- Apr 11, 2022 - iNEMI Webinar 07.07.2021 - PCB Cleaning | ZESTRON Americas
- Jan 28, 2022 - Open Radio Unit White Box 5G | Whizz Systems
- Nov 10, 2021 - Understanding the Cleaning Process for Automatic Stencil Printers | ITW EAE
- Oct 20, 2021 - PCB Surface Finishes & The Cleaning Process - A Compatibility Study | ZESTRON Americas
- Oct 06, 2021 - Cleaning Before Conformal Coating | ZESTRON Americas
- Browse Technical Library »
ALD of Alumina Ceramic Films for Hermetic Protection article has been viewed 557 times